The adverse effects of sea water environment on the fatigue life of woven carbon fiber/vinyl ester composites are established at room temperature in view of long-term survivability of offshore structures. It is observed that the influence of sea water saturation on the fatigue life is more pronounced when the maximum cyclic displacement approaches maximum quasi-static deflection, that is, the reduction in the number of cycles to failure are comparable between dry and sea water saturated samples at lower strain ranges (~37% at 0.46% strain), but are drastically different at higher strain ranges (~90% at 0.62% strain). Key damage modes that manifest during the fatigue loading is also identified, and a non-linear model is established for predicting low cycle fatigue life of these composites in dry and sea water saturated conditions.
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
Pavana Prabhakar, Ricardo Garcia, Muhammad Ali Imam, Vinay Damodaran. 2020-04-06. Flexural Fatigue Life of Woven Carbon/Vinyl Ester Composites under Sea Water Saturation. https://doi.org/10.1016/j.ijfatigue.2020.105641
Cite the original work for its findings. Save a collection to share your selection of sources.