arXiv · 2008.04788
Piezoresistance in defect-engineered silicon
Abstract
The steady-state, space-charge-limited piezoresistance (PZR) of defect-engineered, silicon-on-insulator device layers containing silicon divacancy defects changes sign as a function of applied bias. Above a punch-through voltage ($V_t$) corresponding to the onset of a space-charge-limited hole current, the longitudinal $\langle 110 \rangle$ PZR $\pi$-coefficient is $\pi \approx 65 \times 10^{-11}$~Pa$^{-1}$, similar to the value obtained in charge-neutral, p-type silicon. Below $V_t$, the mechanical stress dependence of the Shockley-Read-Hall (SRH) recombination parameters, specifically the divacancy trap energy $E_T$ which is estimated to vary by $\approx 30$~$\mu$V/MPa, yields $\pi \approx -25 \times 10^{-11}$~Pa$^{-1}$. The combination of space-charge-limited transport and defect engineering which significantly reduces SRH recombination lifetimes makes this work directly relevant to discussions of giant or anomalous PZR at small strains in nano-silicon whose characteristic dimension is larger than a few nanometers. In this limit the reduced electrostatic dimensionality lowers $V_t$ and amplifies space-charge-limited currents and efficient SRH recombination occurs via surface defects. The results reinforce the growing evidence that in steady state, electro-mechanically active defects can result in anomalous, but not giant, PZR.
Explore related subjects
Keep this discovery
H. Li, A. Thayil, C. T. K. Lew, M. Filoche, B. C. Johnson, J. C. McCallum, S. Arscott, A. C. H. Rowe. 2020-08-11. Piezoresistance in defect-engineered silicon. https://doi.org/10.1103/physrevapplied.15.014046
Cite the original work for its findings. Save a collection to share your selection of sources.